17-4PH | 1.4548

1.4548.4 | UNS S17400 | AMS 5622 | AMS 5643 | WL 1.4548.4 | 1.4548.9

The high alloy steel 17-4PH is one of the most commonly used precipitation hardened stainless steels. It contains about 17% chromium and 4% nickel with additions of copper. This type of steel has a martensitic crystalline structure in combination with a very hard and brittle structure that is due to stabilization via precipitation heat treatment. The corrosion resistance of 17-4PH is comparable to that of 304 stainless steel in most media. An excellent combination of high strength and good corrosion resistance at temperatures up to 316°C make this stainless steel extremely versatile and an effective solution for many applications.

 

Areas of application for 17-4PH | 1.4548

Chassis, valves, engine components, molding tools, food processing equipment, chemical processing equipment, refinery equipment, and high strength shafts.

 

Contact us if you have any questions.

S+D METALS Kontakt

17-4PH | Material no. 1.4548.4 

Available from stock in the following dimensions

  • 6,00 mm Ø
  • 8,00 mm Ø
  • 10,00 mm Ø
  • 12,00 mm Ø
  • 14,00 mm Ø
  • 15,00 mm Ø
  • 16,00 mm Ø
  • 18,00 mm Ø
  • 20,00 mm Ø
  • 22,00 mm Ø
  • 25,00 mm Ø
  • 28,00 mm Ø
  • 30,00 mm Ø
  • 32,00 mm Ø
  • 35,00 mm Ø
  • 36,00 mm Ø
  • 40,00 mm Ø
  • 45,00 mm Ø
  • 50,00 mm Ø
  • 55,00 mm Ø
  • 60,00 mm Ø
  • 65,00 mm Ø
  • 70,00 mm Ø
  • 75,00 mm Ø
  • 80,00 mm Ø
  • 85,00 mm Ø
  • 90,00 mm Ø
  • 95,00 mm Ø
  • 100,00 mm Ø
  • 110,00 mm Ø
  • 120,00 mm Ø
  • 130,00 mm Ø
  • 140,00 mm Ø
  • 150,00 mm Ø
  • 160,00 mm Ø
  • 170,00 mm Ø
  • 180,00 mm Ø
  • 190,00 mm Ø
  • 200,00 mm Ø
  • 220,00 mm Ø
  • 250,00 mm Ø

Details at a glance

Chemical composition - limits in %

Fe
Rest
Cr
15,00 - 17,00
Ni
3,00 - 5,00
Cu
3,00 - 5,00
Mn
max. 1,50
Si
max. 0,70
Mo
max. 0,60
Nb
max. 0,45
C
max. 0,07

Physical constants and thermal properties

Density
7.75 g/cm³
Melting point
1404 - 1440 °C
Thermal conductivity at 20°
18.4 W/m - °C
Coefficient of expansion at 21 - 93°C
10.8 μm/m - °C

Typical mechanical properties (at room temperature, Condition H1025)

Yield strength
min. 1000 MPa
Tensile strength
min. 1070 MPa
Elongation
min. 11 %

Downloads

Downloads

Datasheet_17-4PH.pdfDatasheet_17-4PH.pdf